Strength Restoration of The DP Finished Cotton Fabric by Enzymatic Treatment

수지 가공 면직물의 강도 회복을 위한 효소처리 연구

  • Published : 2004.10.01

Abstract

The purpose of this study is restoration for tearing strength of the durable press (DP) finished 100% cotton fabric by enzymatic treatment. Dimethylol Dihydroxy Ethylene Urea (DMDHEU) was used as a DP finish chemical. Enzymes (cellulase, pectinase, protease, lipolase) were selected based on their specific reaction activities. Ideal application of the enzymes for this work was to remove cross-links created by DMDHEU on the surface of the fibers to offer migration property between microstructures of cellulose, yet cross-links that exist inside of the fibers are still remained to impart effect of wrinkle resistance. Physical characteristics (tearing strength, wrinkle recovery, FT-IR) of enzyme treated samples were measured and compared. It was found out that, in case of enzyme treatment, most of enzymes didn't have a great effect on tearing strength, but, in case of Protease, tearing strength increased at DMDHEU 2% treatment. As a result of an experiment on wrinkle recovery of the textiles treated with enzyme making density of DMDHEU different whenever respective experiment was made, it was discovered that density of DMDHEU increased as wrinkle recovery increased and, in the relation to enzyme treatment especially in Lipase enzyme treatment, the lesser density of DMDHEU, the more wrinkle recovery increased.

Keywords