Shrinkage Properties of High Performance Concrete Used Expansive Additive and Shrinkage Reducing Agent

팽창재와 수축저감제를 사용한 고성능 콘크리트의 수축 특성

  • 고경택 (한국건설기술연구원 구조연구부) ;
  • 박정준 (한국건설기술연구원 구조연구부) ;
  • 류금성 (한국건설기술연구원 구조연구부) ;
  • 강수태 (한국건설기술연구원 구조연구부)
  • Received : 2006.01.17
  • Accepted : 2006.02.13
  • Published : 2006.07.31

Abstract

Generally, high performance concrete has characteristics such as low water-cementitious material ratio, lots of unit binder powder, thus the heat of hydration, autogenous shrinkage are tend to be increased. This study is to investigated the effect of the expansive additive and shrinkage reducing agent on the shrinkage properties of high performance concrete as a study to develop the reduction technology of the concrete shrinkage. Test results showed that the expansive additive and shrinkage reducing agent were effective the reduction of shrinkage of high performance concrete. Especially, the using method in combination with expansive additive and shrinkage reducing agent was more effective than the separately using method of that. Also, it analyzed that the combination of expansive additive of 5% and shrinkage reducing agent of 1% was the most suitable mixture, considering to the fluidity, strength and shrinkage properties.

고성능 콘크리트는 물-결합재비를 작게 하고, 단위결합재량을 다량으로 사용하므로 콘크리트의 수화열 및 자기수축이 증대되는 경향이 있다. 본 연구에서는 고성능 콘크리트의 수축저감 기술을 구축하는 연구의 일환으로 팽창재와 수축저감제 사용이 고성능 콘크리트의 수축특성에 미치는 영향을 검토하였다. 그 결과, 팽창쟁와 수축저감제는 고성능 콘크리트의 수축을 저감시키는 데 효과가 뛰어나며, 특히 팽창재와 수축저감제를 조합하여 사용할 경우, 각각 단독으로 사용하는 경우보다는 수축 저감 효과가 큰 것으로 확인되었다. 또한 시공성, 강도 및 수축특성을 종합적으로 고려하여 팽창재 5.0%와 수축저감제 1.0%의 조합이 적정배합으로 분석되었다.

Keywords

References

  1. 고경택, 박정준, 김방욱, 김성욱, 이장화(2002) 광물질 혼화재료를 사용한 고성능콘크리트의 자기수축. 2002년도 학술발표회, 대한토목학회
  2. 고경택, 박정준, 김성욱, 이장화(2004) 고성능콘크리트의 자기수축 저감에 관한 실험적 연구. 대한토목학회논문집, 대한토목학회, 제24권 제3-A호, pp. 501-508
  3. 유성원, 김도겸, 고경택, 정상화(2004) 수축저감제 및 팽창재가 혼입된 고성능콘크리트의 자기수축 모델에 관한 연구. 대한토목학회논문집, 대한토목학회, 제24권 제6-A호, pp. 1301-1307
  4. 한천구, 반호용, 전병채, 홍상희(1992) CSA계 팽창재 및 무기질 혼화재를 이용한 고성능 콘크리트의 특성에 관한 연구. 한국콘크리트학회논문집, 한국콘크리트학회, Vol. 11, No. 1, pp. 141-148
  5. 近藤直孝, 大門正機(2000) セメント系膨脹材を混和したセメントの水和反應と膨脹機構. コンクリ-ト工學年次論文集, 日本コンクリ-ト工學協會, Vol. 22, No. 2, pp. 25-30
  6. 盛岡實, 秋原宏俊, 大門正機(1998) カルシウムサルホアルミネ-ト系膨脹材の水和におよぼす$C_{3}$Aと二水セッコウの影響. セメント一コンクリ-ト論文集, 日本セメント協會, No. 52, pp. 2-7
  7. 自己收縮硏究委員(2002) コンクリ-トの自己收縮硏究委員會報告書, 日本コンクリ-ト工學協會
  8. Berke, N.S., Dallarire, M.P., Hicks, M.C., and Kerkar, A. (1997) New development in shrinkage-reducing admixtures. Proceedings of Fifth CANMET/ACI International Conference on Superplasticizers and Other Chemical Admixtures in Concrete, Rome, ltaly, ACI SP-173, pp. 971-998
  9. De Larrard, F. and Le Roy, R. (1992) The influence of mix composition on mechanical properties of high-performance silicafume concrete. Proceedings of the 4th CANMET/ACI International Conference on Fly Ash, Silica Fume. Slag and Natural Pozzolans in Concrete, ACI SP-132, pp. 965-986
  10. Enyi, C. and Huizhen, L. (1999) Role of expansive admixtures in high-performance concrete. High-Performance Concrete : Research to Practice, ACI SP-189, pp. 575-587
  11. Nagataki, S. and Gomi, H. (1998) Expansive admixture (mainly ettringite). Cement and Concrete Composite, No. 20. pp. 163-170 https://doi.org/10.1016/S0958-9465(97)00064-4
  12. Shah, S.P., Karaguler, M.E., and Sarigaphuti, M. (1992) Effects of shrinkage-reducing admixtures on restrained shrinkage cracking of concrete. ACI Materials Journal, Vol. 89, No. 3. pp
  13. Tazawa, E. and Miyazawa, M. (1995) Experimental study on mechanism of autogenous shrinkage of concrete. Cement and Concrete Research, Vol. 25, No. 8, pp. 1633-1638 https://doi.org/10.1016/0008-8846(95)00159-X