Effect of metal primer and thermocycling on shear bonding strength between the orthodontic bracket and gold alloy

치과용 금합금에 대한 금속 프라이머 처리와 열순환 처리가 교정용 브라켓의 전단결합강도에 미치는 영향

  • Lee, Young-Kee (Department of Orthodontics, College of Dentistry, Yonsei University) ;
  • Cha, Jung-Yul (Department of Orthodontics, College of Dentistry, Yonsei University) ;
  • Yu, Hyung-Seog (Department of Orthodontics, College of Dentistry, Oral Science Research Institute, The Institute of Cranio-facial Deformity, Yonsei University) ;
  • Hwang, Chung-Ju (Department of Orthodontics, College of Dentistry, Oral Science Research Institute, The Institute of Cranio-facial Deformity, Yonsei University)
  • 이영기 (연세대학교 치과대학 교정학교실) ;
  • 차정열 (연세대학교 치과대학 교정학교실) ;
  • 유형석 (연세대학교 치과대학 교정학교실, 두개안면기형 연구소, 구강과학연구소) ;
  • 황충주 (연세대학교 치과대학 교정학교실, 두개안면기형 연구소, 구강과학연구소)
  • Received : 2009.03.30
  • Accepted : 2009.08.16
  • Published : 2009.10.30

Abstract

Objective: The aim of this study was to evaluate the effect of metal primers and thermocycling on shear bond strength between the orthodontic bracket and gold alloy. Methods: For this study, 80 specimens made of dental gold alloy were divided into 8 groups based on the combination of metal primers (none, Alloy primer, Metaltite, V-primer) and thermocycling (with and without thermocycling). Shear bond strength testing was performed with a universal testing machine. Bond failure sites were classified by a modified ARI (Adhesive Remnant Index) score. Results: All metal primer treated groups showed a significantly higher shear bond strength than the only sandblasting treated group without thermocycling (p < 0.05). There were no significant differences on shear bond strength in the groups with thermocycling (p > 0.05). Bond failure sites of the metal primer treated group without thermocycling occurred at gold alloy/adhesive interface, whereas there were no differences on bonding failure sites in the groups with thermocycling. Conclusions: These findings suggest that using metal primer on gold alloy enhances the initial bracket bond strength. But, this effect was not shown with thermocycling.

치과용 금합금에 교정용 브라켓 접착 시 금속 프라이머와 열순환 처리가 전단결합강도에 미치는 영향을 알아보기 위하여 80개의 치과용 금합금 시편을 샌드블라스팅만 처리한 군과 3종류의 금속 프라이머(Alloy Primer, Metaltite, V-Primer)처리를 시행한 군으로 분류하고, 이를 열순환 처리 시행 여부에 따라 모두 8개 군으로 분류하였다. 만능물성 시험기를 사용하여 브라켓의 전단결합강도를 측정하고, modified ARI (Adhesive Remnant Index) scores를 통해 브라켓 접착면의 파절 양상을 평가하였다. 열순환 처리 미시행 시에는 금속 프라이머의 적용 시 샌드블라스팅만 단독으로 처리한 경우에 비하여 통계적으로 유의성 있는 전단결합강도의 증가가 있었다 (p < 0.05). 열순환 처리를 시행한 군에는 금속 프라이머의 처리에 의한 전단결합강도의 변화는 유의한 차이가 없었다 (p > 0.05). 금속 프라이머를 적용한 경우 열순환 처리 미시행 시에는 파절 양상이 브라켓과 접착제 계면에서의 파절 발생 빈도가 높았으나, 열순환 처리 시행 시에는 각 군 간 파절 양상에 유의한 차이가 없었다. 이상의 결과로 금속 프라이머의 적용이 치과용 금합금에 대한 교정용 브라켓 접착 시 초기 접착 강도에서는 유의성 있는 결합력의 증가를 보이나, 열순환 처리 시행 후에는 결합 강도에서는 유의한 차이가 없는 것으로 나타나 금속 프라이머에 의한 결합력 증가가 감소하는 것으로 생각한다.

Keywords

References

  1. Yu HS, Ryu YK, Lee JY. A study on the distributions and trends in malocclusion patients from Department of Orthodontics, College of Dentistry, Yonsei University. Korean J Orthod 1999;29:267-76
  2. Buonocore MG. A simple method of increasing the adhesion of acrylic filling materials to enamel surfaces. J Dent Res 1955;34:849-53 https://doi.org/10.1177/00220345550340060801
  3. Newman GV. Epoxy adhesives for orthodontic attachments: progress report. Am J Orthod 1965;51:901-12 https://doi.org/10.1016/0002-9416(65)90203-4
  4. Keim RG, Gottlieb EL, Nelson AH, Vogels DS 3rd. 2002 JCO study of orthodontic diagnosis and treatment procedures. Part 1. Results and trends. J Clin Orthod 2002;36:553-68
  5. Boyd RL, Baumrind S. Periodontal considerations in the use of bonds or bands on molars in adolescents and adults. Angle Orthod 1992;62:117-26
  6. Proffit WR, Fields HW, Sarver DM. Contemporary orthodontics. 4th ed. St. Louis: Mosby Elsevier; 2007. p. 658-9
  7. Wood DP, Jordan RE, Way DC, Galil KA. Bonding to porcelain and gold. Am J Orthod 1986;89:194-205 https://doi.org/10.1016/0002-9416(86)90032-1
  8. Andreasen GF, Stieg MA. Bonding and debonding brackets to porcelain and gold. Am J Orthod Dentofacial Orthop 1988;93: 341-5 https://doi.org/10.1016/0889-5406(88)90164-3
  9. Büyükyilmaz T, Zachrisson YO, Zachrisson BU. Improving orthodontic bonding to gold alloy. Am J Orthod Dentofacial Orthop 1995;108:510-8 https://doi.org/10.1016/S0889-5406(95)70051-X
  10. Graber TM, Vanarsdall RL, Vig KWL. Orthodontics: current principles and techniques. 4th ed. St. Louis: Elsevier Mosby; 2005. p. 596-602
  11. Gale MS, Darvell BW. Thermal cycling procedures for laboratory testing of dental restorations. J Dent 1999;27:89-99 https://doi.org/10.1016/S0300-5712(98)00037-2
  12. Bishara SE, Ajlouni R, Laffoon JF. Effect of thermocycling on the shear bond strength of a cyanoacrylate orthodontic adhesive. Am J Orthod Dentofacial Orthop 2003;123:21-4 https://doi.org/10.1067/mod.2003.1
  13. Artun J, Bergland S. Clinical trials with crystal growth conditioning as an alternative to acid-etch enamel pretreatment. Am J Orthod 1984;85:333-40 https://doi.org/10.1016/0002-9416(84)90190-8
  14. Zachrisson BU. Orthodontic bonding to artificial tooth surfaces: clinical versus laboratory findings. Am J Orthod Dentofacial Orthop 2000;117:592-4 https://doi.org/10.1016/S0889-5406(00)70211-3
  15. Kojima K, Kadoma Y, Imai Y. Adhesion to precious metals utilizing triazine dithione derivative monomer. J Jpn Dent Mater 1987;6:702-7.
  16. Suzuki M, Fujishima A, Miyazaki T, Hisamitsu H, Kojima K, Kadoma Y. A study on the adsorption structure of an adhesive monomer for precious metals by surface-enhanced Raman scattering spectroscopy. Biomaterials 1999;20:839-45 https://doi.org/10.1016/S0142-9612(98)00238-5
  17. Ryou DB, Kwon TY, Kwon YH, Kim KH. An effect priming gold alloy on bonding to orthodontic bracket. J Korean Res Soc Dent Mater 2003;30:347-56
  18. Yanagida H, Matsumura H, Atsuta M. Bonding of prosthetic composite material to Ti-6Al-7Nb alloy with eight metal conditioners and a surface modification technique. Am J Dent 2001;14:291-4
  19. Tanaka T, Fujiyama E, Shimizu H, Takaki A, Atsuta M. Surface treatment of nonprecious alloys for adhesion-fixed partial dentures. J Prosthet Dent 1986;55:456-62 https://doi.org/10.1016/0022-3913(86)90176-9
  20. Sparrius O, Grossman ES. Marginal leakage of composite resin restorations in combination with dentinal and enamel bonding agents. J Prosthet Dent 1989;61:678-84 https://doi.org/10.1016/S0022-3913(89)80041-1
  21. Kang SW, Son WS, Park SB, Kim SS. Effect of thermocycling on shear bond strength and mode of failure of ceramic orthodontic brackets bonded to different porcelain restorations. Korean J Orthod 2009;39:225-33 https://doi.org/10.4041/kjod.2009.39.4.225
  22. Atsuta M, Matsumura H, Tanaka T. Bonding fixed prosthodontic composite resin and precious metal alloys with the use of a vinyl-thiol primer and an adhesive opaque resin. J Prosthet Dent 1992;67:296-300 https://doi.org/10.1016/0022-3913(92)90233-Z
  23. Matsumura H, Shimoe S, Nagano K, Atsuta M. Effect of noble metal conditioners on bonding between prosthetic composite material and silver-palladium-copper-gold alloy. J Prosthet Dent 1999;81:710-4 https://doi.org/10.1016/S0022-3913(99)70111-3
  24. Yoshida K, Atsuta M. Effect of MMA-PMMA resin polymerization initiators on the bond strengths of adhesive primers for noble metal. Dent Mater 1999;15:332-6 https://doi.org/10.1016/S0109-5641(99)00053-6
  25. Reynolds IR. A review of direct orthodontic bonding. Br J Orthod 1975;2:171-8

Cited by

  1. Light emitting diode를 이용한 광중합 시 금합금과 교정용 금속 브라켓의 전단접착강도 vol.40, pp.1, 2009, https://doi.org/10.4041/kjod.2010.40.1.27
  2. Image Quality of the 3 Dimensional Phase-Contrast Technique in an Intracranial Magnetic Resonance Angiography with Artifacts Caused by Orthodontic Devices: A Comparison with 3 Dimensional Time-of-Flig vol.65, pp.1, 2009, https://doi.org/10.3348/jksr.2011.65.1.1