A study on the corrosion control of tap water by lime and carbon dioxide

소석회와 이산화탄소를 이용한 수돗물 부식성 제어에 관한 연구

  • Published : 2011.04.15

Abstract

A method to improve internal corrosion control efficiency by adding lime and carbon dioxide, which, in turn increases the Langelier Index (LI) for filtered water at a conventional drinking water treatment plant (WTP) was investigated. The SJ WTP (Q=100,000 $m^{3}$/d) has been operating an internal corrosion control system since 2006. The system has achieved stable operation through technical development and trial and error over a period of several years. As a result of the operation, the LI of treated water has increased up to 29% by adjusting pH of filtered water to 7.8 with the addition of lime and carbon dioxide. Coupon tests in the distribution system indicated that the corrosion rate has been delayed by 24% when the internal corrosion method was implemented. The increase of LI by lime and carbon dioxide has been proven to be a practical method for controlling corrosion.

Keywords

References

  1. 구성은, 우달식, 이두진, 김주환, 안효권, 문광순 (2006) 수질제어 및 부식억제제에 의한 상수도관의 내부부식 제어, 상하수도학회지, 20(2), pp.215-223.
  2. 국립환경과학원 (2009) 수도관 노후방지를 위해 부식성 관리필요, 보도자료.
  3. 김성일, 우달식, 남상호, 박영복 (2006) 소석회와 $Co_{2}$로 안정화된 수돗물의 부식제어 효과, 대한환경공학회 춘계학술발표회논문집, pp.1067-1069.
  4. 김진근, 이송희, 김재원 (2010) 급속여과공정에서 여과수질 저하 원인 및 개선방안, 상하수도학회지, 24(3) pp.333-339.
  5. 이현동, 곽필재, 이지은, 김영관 (2009) 상수도관망 시스템의 부식 제어를 위한 수질모니터링, 상하수도학회지, 23(1), pp.77-87.
  6. 정원석, 김태훈, 이재희 (2009) 분말소석회와 이산화탄소를 이용한 관내부식 제어설비 운영사례 연구, 상하수도학회 추계 학술발표회 논문집, pp.223-224.
  7. 환경부 (2011) 먹는물 수질관리 지침.
  8. 황병기, 우달식 (2009) 상수원수의 부식평가 지수 산정 프로그램 개발 및 탄산칼슘 포화지수에 의한 수돗물의 부식성 평가, 한국산학기술학회논문지, 10(4), pp.177-185.
  9. AWWA (1986) Corrosion control for operators.
  10. K-water (2010) 정수처리시설 종합개선계획 보완, pp.V-100-107.
  11. Schock, M.R. (1999) Internal corrosion and deposition control in Water Quality and Control 5th Ed. AWWA. 1999.