Reliability Evaluation of ER Type Corrosion Sensor for Monitoring Corrosion of Piping System Under Accelerated Corrosion Environment

배관의 부식 상태 진단에 사용되는 ER 부식센서의 가속부식환경에서의 신뢰성 평가

  • Hwang, Hyun-Kyu (Graduate School, Mokpo National Maritime University) ;
  • Shin, Dong-Ho (Graduate School, Mokpo National Maritime University) ;
  • Kim, Heon-Hui (Division of Marine Engineering, Mokpo National Maritime University) ;
  • Lee, Jung-Hyung (Division of Marine Engineering, Mokpo National Maritime University)
  • 황현규 (목포해양대학교 대학원) ;
  • 신동호 (목포해양대학교 대학원) ;
  • 김헌희 (목포해양대학교 기관시스템공학부) ;
  • 이정형 (목포해양대학교 기관시스템공학부)
  • Received : 2021.11.21
  • Accepted : 2021.11.26
  • Published : 2021.12.31

Abstract

In this study, the reliability of a commercial ER-type corrosion sensor was evaluated under an accelerated corrosion environment to verify its suitability for application in monitoring of ship's seawater piping system. A closed-loop pump piping testbed was designed and constructed to compare the wall thickness reduction of the pipe and the response from the sensor. The sensor was attached inside the pipe near the outlet of the pump that was exposed to a 3.5% NaCl solution with or without copper accelerated acetic acid (CASS). The results demonstrated that the presence of CASS significantly increased the corrosivity of the solution as well as the thickness reduction of the pipe, as expected. On the other hand, the corrosion products formed by the solution with CASS were thicker compared with those without CASS. The sensor response to temperature variation was found to be a clear linear relationship for the solution without CASS but there was a non-linear relationship where CASS was present.

Keywords

Acknowledgement

This work was supported by the 'Autonomous Ship Technology Development Program (2001-1164, Development of Performance Monitoring and Failure Prediction and Diagnosis Technology for Engine System of Autonomous Ships)' funded by the Ministry of Trade, Industry & Energy (MOTIE, Korea).

References

  1. Julio C. Adamowski, Flavio Buiochi, Marcos Tsuzuki, Nicolas Perez, Claudio S. Camerini and Carlos Patusco, Ultrasonic measurement of micrometric wall-thickness loss due to corrosion inside pipes, IEEE, p. 1181 (2013). Doi: https://doi.org/10.1109/ULTSYM.2013.0479
  2. Faisal Durrani, Ryan Wesley, Vijay Srikandarajah, Mahroo Eftekhari and Steve Munn, Predicting Corrosion rate in Chilled HVAC Pipe Network: Coupon vs Linear Polarisation Resistance method, Engineering Failure Analysis, 109, 1 (2020). Doi: https://doi.org/10.1016/j.engfailanal.2019.104261
  3. Zheng Liu and Yehuda Kleiner, State-of-the-Art Review of Technologies for Pipe Structural Health Monitoring, IEEE, 12, 1987 (2012). Doi: https://doi.org/10.1109/JSEN.2011.2181161
  4. ASTM B368-97, Standard Test Method for Copper-Accelerated Acetic Acid-Salt Spray (Fog) Testing (CASS Test), p. 1 (2003).
  5. J. H. Lee, K. H. Jung, J. C. Park and S. J. Kim, Determination of optimum protection potential for cathodic protection of offshore wind-turbine-tower steel substructure by using potentiostatic method, Journal of the Korean Society of Marine Engineering, 41, 230 (2017). Doi: https://doi.org/10.5916/jkosme.2017.41.3.230
  6. Y. Bai and Q. Bai, Subsea Engineering Handbook, 2nd Edition, p. 464, Gulf Professional Publishing (2019). https://www.elsevier.com/books/subsea-engineeringhandbook/bai/978-0-12-812622-6
  7. ASTM G102-89, Standard Practice for Calculation of Corrosion Rates and Related Information from Electrochemical Measurements, p. 1 (2004).
  8. Yu Zuo, Haitao Wang, Jingmao Zhao and Jinping Xiong, The effects of some anions on metastable pitting of 316L stainless steel, Corrosion Science, 44, 13 (2002). Doi: https://doi.org/10.1016/S0010-938X(01)00031-2
  9. N. Voevodin, C. Jeffcoate, L. Simon, M. Khobaib and M. Donley, Characterization of pitting corrosion in bare and sol-gel coated aluminum 2024-T3 alloy, Surface and Coatings Technology, 140, 29 (2001). Doi: https://doi.org/10.1016/S0257-8972(01)01000-3
  10. H. K. Hwang and S. J. Kim, Effect of Temperature on Electrochemical Characteristics of Stainless Steel in Green Death Solution Using Cyclic Potentiodynamic Polarization Test, Corrosion Science and Technology, 20, 266 (2021). Doi: https://doi.org/10.14773/cst.2021.20.5.266
  11. Dooho Choi and Sung-il Seo, Evaluation of Corrosion Behavior of Railway Axle Material (RSA1) in Seawater, Journal of the Korea Academia-Industrial cooperation Society, 16, 5039 (2015). Doi: https://doi.org/10.5762/KAIS.2015.16.8.5039
  12. M. J. Kim, D. J. Kim and H. P. Kim, Manufacture of magnetite (Fe3O4) electrode and its electrochemical properties, Corrosion Science and Technology, 14, 19 (2015). Doi: https://doi.org/10.14773/cst.2015.14.1.19
  13. J. H. Lee, J. C. Park, M. S. Han, S. K. Jang and S. J. Kim, Influence of Current Density Application Time on the Corrosion Damage of Offshore Wind SteelSubstructure in Galvanostatic Corrosion Experiment, Journal of The Korean Institute of Surface Engineering, 49, 431 (2016). Doi : http://www.dbpia.co.kr/journal/articleDetail?nodeId=NODE07047285 https://doi.org/10.5695/JKISE.2016.49.5.431